  今天工业电源小编来和大家说一下给蓄电池添加电解液或水时需要注意的几点要求:
  电解液高过极板10至15毫米即可;有两条红线的蓄电池,电解液不得超过上红线。电解液太满会从蓄电池盖小孔中溢出。电解液导电,一旦流到蓄电池正、负两极之间,就会形成回路自放电。遇此情况就应将电解液擦掉,或用开水冲洗擦净。
  加电解液时若有东西不慎掉入,千万不能用金属物去捞,应用木棒夹出杂质;如用铁丝或铜丝去捞,金属分子会在硫酸的腐蚀下进入蓄电池形成自放电,而损坏蓄电池。
  蓄电池在充放电过程中,电解液中的水会因为电解和蒸发而逐渐减少,导致电解液面下降。如果不及时补充的话,有可能缩短蓄电池的使用寿命,应及时补充蒸馏水,切忌用饮用纯净水代替。因为纯净水中含有多种微量元素,对蓄电池会造成不良影响。
  Industrial power supply small make up today and everyone said once to add battery electrolyte or water need to be aware of some requirements:
  The electrolyte is higher than plate 10 to 15 mm;There are two red line of the battery, the electrolyte must not exceed the red line.The electrolyte is too full can overflow from the battery cover holes.Conductive, once the electrolyte flow into the battery between positive and negative poles of self-discharge will form a loop.In this situation is the electrolyte should be erased, or rinse wipe with boiled water.
  And if something accidentally fell into the electrolyte, scoop, never use a metal to stick clip out impurities;Such as wire or copper wire to scoop, metal molecules will under the corrosion of sulphuric acid into the battery self-discharge formation, and damage the battery.
  Battery in the process of charging and discharging, the water in the electrolyte will gradually reduce by electrolysis and evaporation, led to the decrease of the electrolytic liquid level.If not timely supplement, may shorten the service life of the battery, should be timely replenish distilled water, avoid by all means is replaced with drinking water.Because water is contained in a variety of trace elements, the battery can cause bad influence.